A 5,000 hour xenon hollow cathode life test

John Brophy, Charles Garner

27th Joint Propulsion Conference · 1991 · 23 citations · 16 references

Concepts

Abstract

A cathode life test voluntary terminated after 5024 hours of operation at 25 A is reported. The cathode including a 6.35-mm diameter by 57.12-mm long molybdenum tube with a nominal wall thickness of 0.38 mm is described along with a test facility and start-up procedure. It is shown that over the time of the experiment, the cathode-orifice diameter eroded from 1.80 mm to 2.08 mm, which corresponds to a ratio of the emission current to the orifice diameter at the end of the test of 12.0 A/mm. Tungsten deposits on the interior surface of the insert are detected in post-test analyses, and complete depletion of the original impregnate is suggested by X-ray diffraction analyses. A cathode-jet phenomenon in which energetic ions are produced during hollow-cathode operation at emission currents above 20 A is confirmed.