The Journal of Indian Prosthodontic Society · 2012 · 18 citations · 29 references
Natural SciencesMaterials EngineeringMaterials ScienceDental MaterialsMechanical Behavior Of MaterialsPolymer MaterialsComposite MaterialsFiber-reinforced CompositesFlexural PropertiesPolymer CompositesStrength Of MaterialsStrength PropertiesFiber ReinforcementFiber Reinforcement EffectsFlexural StrengthGlass Fiber Reinforced CompositesGlass Fiber ReinforcementPolymethyl MethacrylateProvisional Restoration MaterialsRestorative Materials
The aim is to evaluate and compare the flexural strength of different provisional restorative materials reinforced with glass and polyethylene fibers. A total of 90 samples were prepared and divided into three groups based on the type of fiber reinforcement, unidirectional S-glass (Splint-It) and ultra-molecular weight polyethylene (Ribbond). Unreinforced samples served as control group. Again each group was subdivided into three subgroups based on type of provisional restorative resins, heats cure polymethyl methacrylate, self-cure poly methyl methacrylate and self-cure bis-acryl composite. Samples were loaded in a universal testing machine until fracture occurs. The mean flexural strengths (MPa) were subjected to the one-way ANOVA, followed by the Tukey-HSD test at a significance level of 0.001. The result shows all the fiber reinforced samples possessed greater strength than the control samples. In control samples, the heat cure poly methyl methacrylate resin (72.74 ± 2.28 MPa) had the greatest flexural strength, followed by self-cure bis-acryl composite (67.05 ± 2.35 MPa) and self-cure poly methyl methacrylate resin (52.88 ± 1.90 MPa). In both heat and self-cure poly methyl methacrylate resin, the polyethylene fiber reinforcement (96.00 ± 2.63 MPa, 86.17 ± 1.92 MPa) provides the greatest strength than glass fiber reinforcement (92.68 ± 1.58 MPa, 76.40 ± 2.11 MPa). In self-cure bis-acryl composite, the glass fiber (105.95 ± 3.07 MPa) shows better reinforcement than polyethylene fiber (99.41 ± 1.74 MPa).The fibers reinforcement increases the flexural strength of provisional restorative resins.
29