Modern Applied Science · 2011 · 11 citations · 9 references
EngineeringMaterials EngineeringMaterials ScienceMaterials CharacterizationMechanical Behavior Of MaterialsMetallurgyAlloysCladding MaterialsLaser Material ProcessingLaser Surface ProcessingPowder MetallurgyPowder ProcessingLaser Beam MachiningLaser CladdingLaser MaterialsLaser Metal DepositionMetal PowdersNi-al Alloys
In this study, continuous wave CO2 laser with 1.7 and 2 kW were used to deposit clad layers of premixed powders of either Ni-10 wt% Al or Ni-30 wt% Al onto inconel 617 substrate. Different cladding traverse speeds in the range 1 to 35 mm/s were used for premixed clad powder of Ni-10 wt% Al and 1.65 to 11.2 mm/s for premixed clad powder of Ni-30 wt% Al. Two powder feeding rates were used, 10 and 8.9 gm/min for premixed clad powders of Ni-10 wt% Al and Ni-30 wt% Al respectively. The other laser independent variables were selected to be constant. The results showed that different percentages of area dilution were found ranging from 3.7 to 78.3% for premixed clad powder of Ni-10 wt% Al and 6.9 to 41 % for premixed clad powder of Ni-30 wt% Al depending on the laser cladding independent variables used. Furthermore, dilution was affected mainly by cladding traverse speeds.
9
Stimulated Optical Radiation in Ruby
Theodore H. Maiman · Nature · 1960 · 4.8K citations
High-Power Laser Beam Cladding
G. J. Bruck · JOM · 1987 · 33 citations