Very regularly coiled spring-like fibers of Si3N4 have been obtained from a gas mixture of Si2Cl6, NH3, and H2 at 1200 °C on a graphite substrate on which an iron impurity was painted. The spring-like fibers were amorphous Si3N4 with a circular cross section having a 0.5–1 μm thickness, 3–5 μm coil pitch, 10–15 μm coil diameter, and 50–100 μm coil length. The height of the bush of the fibers reached 1.5–2 mm after 30 min reaction time.