Applied Physics Letters · 1988 · 21 citations · 11 references
EngineeringMaterials EngineeringMaterials ScienceMechanical Behavior Of MaterialsMetallurgyTribologyAlloysIon ImplantationSteel MaterialsStrengthening MechanismsWear ResistanceWear-resistant MaterialsAnti-wear PerformanceBrittle FailureCompressive StrainStrengtheningWear RatesWear Resistance EnhancementWear Resistance ImprovementWear-resistant Alloys
In general, neon implantation is not very effective in reducing wear rates. However, neon implantation into laser-melted steel turns out to reduce the wear rate substantially as a result of a conversion of residual tensile stresses into compressive ones. Nitrogen implantation, on the other hand, at a high dose of 3×1017 ions/cm2 at 90 °C exhibits a deleterious effect on the wear performance. A brittle layer of ε-Fe2(C,N)1−x nitrides is formed. At a lower dose of 1×1017/cm2 or implantation of nitrogen at 150 °C, the wear rate is also reduced.
11
Ion implantation into metals and cabrides
G. Dearnaley, N. E. W. Hartley · Thin Solid Films · 1978 · 126 citations
Natural Sciences, Materials Engineering, Materials Science +10
Nitrogen implantation into steels
N. Moncoffre · Materials Science and Engineering · 1987 · 45 citations
Mechanical state of laser melted surfaces
Michael R. James, D. S. Gnanamuthu, R. J. Moores · Scripta Metallurgica · 1984 · 40 citations