Journal of Oral Rehabilitation · 2004 · 40 citations · 24 references
DentistryDental Biomaterials ScienceDental Materials ScienceDental MaterialsMechanical Properties Of Dental MaterialsProsthodontic MaterialsAll-ceramic RestorationsCeramic RestorationsDental CeramicsDental CompositesFracture ResistancePost RestorationsCeramic Crown SystemsCeramic PostsFracture Resistance Of RestorationsGlass Fiber Reinforced CompositesMaterial ReinforcementPost Fracture ResistanceTitanium MaterialsTitanium Posts
The aim of this in vitro study was to compare the fracture resistance and marginal adaptation of all-ceramic incisor crowns with all-ceramic posts, glass-fibre-reinforced posts and titanium posts as well as a control without any post. Three groups of eight maxillary incisors were restored with an all-ceramic post, a fibre-reinforced composite (FRC) post, a titanium post and a further group was restored without posts. Composite cores were provided and all-ceramic crowns were adhesively luted. After artificial ageing, the fracture resistance of the restored teeth was determined. The marginal adaptation of the restorations at the interfaces between cement-tooth and cement-crown was evaluated with scanning electron microscopy using replica specimen before and after ageing. The restored teeth without posts [270N (235/335)] showed no significantly different fracture strength compared with teeth with the titanium system [340N (310/445)]. The all-ceramic posts [580N (425/820)] and the FRC posts [505N (500/610)] both provided a significant higher fracture resistance than the teeth without posts. Prior to ageing, all materials showed <5% separation at the margins cement-tooth or cement-crown ('marginal gap'). After ageing, the interfaces of all systems deteriorated to values between 6 and 14% marginal gap. The greatest marginal gap was found with the titanium system (14%) at the interface cement-crown and with the all-ceramic posts (12%) at the transition between cement-tooth. Regarding fracture resistance and the marginal adaptation, the all-ceramic and FRC posts may be considered as an alternative to the commonly used titanium post restorations.
24
Guido Heydecke, Frank Butz, Jörg Rudolf Strub · Journal of Dentistry · 2001 · 266 citations
Stavros Kiliaridis, Heidrun Kjellberg, Bengt Wenneberg et al. · Acta Odontologica Scandinavica · 1993 · 260 citations · Full text