Critical pitting potentials for the binary Cr-Fe and Cr-Ni alloys in 0.1N NaC1 become more noble (correspondingly more resistant o pitting) with in-creasing Cr content, particularly in the region 25-40 % Cr and 10-20 % Cr, re-spectively. The potentials for 57.8 % Cr-Fe and pure Cr fall within the trans-passive region. Ni containing 3.2 % Mo, to the contrary, shows a lower (more active) critical potential; higher per cent Mo-Ni alloys appear to fall within the transpassive region corroding anodically as MOO4-- plus Ni + + without pitting. Ni alloyed with 15 % Cr-Fe shifts the potential in the noble direction; Mo alloyed with 15 % Cr, 13 % Ni stainless steel has a similar but even greater effect. At 0 ~ 15 % Cr, 13 % Ni stainless teel exhibits a potential 0.5v more noble than at 25 ~ corresponding to greatly increased resistance to pitting. This shift is less pronounced for the stainless steels containing Mo; in fact, at or above 1.5 % Mo, the critical potentials at 0 ~ are below those at 25 ~ In 0.1N NaBr, alloyed Mo shifts the potentials l ightly in the active di-