Enhanced Thermal Stability and Oxygen Storage Capacity for Ce<i><sub>x</sub></i>Zr<sub>1-</sub><i><sub>x</sub></i>O<sub>2</sub> (<i>x</i> = 0.4−0.6) Solid Solutions by Hydrothermally Homogenous Doping of Trivalent Rare Earths

Rui Si, Ya‐Wen Zhang, Limin Wang, Shijie Li, Bingxiong Lin, Wangsheng Chu, Ziyu Wu, Chun‐Hua Yan

The Journal of Physical Chemistry C · 2006 · 89 citations · 43 references

Concepts

Abstract

Trivalent rare-earth (RE = La, Pr, Nd, Y)-doped Ce x Zr 1- x O 2 ( x = 0.4−0.6) solid solutions were synthesized via a urea hydrolysis-based hydrothermal method, followed by calcination at 1000 °C for 100 h. The X-ray absorption near-edge structure (XANES) tests for the Ce LIII edge determine that the chemical valence of the Ce atom in either undoped or RE-doped CeO 2 −ZrO 2 samples was mainly +4. The measurements of X-ray fluorescence (XRF) and energy-filtered transmission electron microscopy (EFTEM) testify to the good compositional homogeneity for Ce, Zr, and RE atoms in both bulk and microdomain of the as-calcined Ce x Zr 1- x - y RE y O 2- z ( x = 0.4−0.6, y = 0−0.16, and z is the number of oxygen vacancy) samples. The characterizations with X-ray diffraction (XRD) and vis-Raman demonstrate the high structural homogeneity for ternary CeO 2 −ZrO 2 −RE 2 O 3 solid solutions after calcination at 1000 °C for 100 h. The aliovalent substitution of the RE 3+ ion for the Ce 4+ or Zr 4+ ion has been concluded to stabilize the pseudo cubic t ‘ ‘ -structure, to improve the surface area and to enhance the oxygen storage capacity (OSC) for the binary CeO 2 −ZrO 2 system. The reducibility of the as-calcined Ce x Zr 1- x - y RE y O 2− z by CO seems dependent upon the nature and concentration of the RE dopant. The highest CO−OSC value obtained in this work appeared for Ce 0.5 Zr 0.42 Nd 0.08 O 2- z in 558 μmol CO g -1 at 700 °C, while the undoped samples gave a value of less than 460 μmol CO g -1 .

References

43