Prevention of Red Scale Formation during Hot Rolling of Steels.

Hikaru OKADA, Tomoki Fukagawa, Haruhiko Ishihara, Atsuki Okamoto, Masatoshi Azuma, Yukio Matsuda

ISIJ International · 1995 · 60 citations · 0 references

DOIFull text

Open access

Concepts

Abstract

Redscale defects usually observed in high Si hot rolled strip were reproduced in a laboratory 3 stand tandem mill. The effects of hot rolling and descaling conditions on the strip surface color and scale structure were examined. lrrespective of Si content in steel. the hot rolled strip surface becamered when the scale thickness before rolling was above 20,tm and the rolling temperature was below 900'C. It was found that surface part of the scale (mainly FeO) was broken to powderby hot rolling at the temperature below 900"C. The red scale of Fe.O, was formed by the oxidation of powderedscale during cooling. Thick scale formed during slab soaking was completely removed by hydraulic descaling before rolling in low Si steel, whereas that was not removed in high Si steel. This remained scale caused the red sca]e defects after rolling and cooling. The application of obtained results to the hot strip mill production of red scaleless strip was discussed.