Onset of Hot Tearing in AE42 Magnesium Alloy

Lukas Bichler, C. Ravindran, D. Sediako

Canadian Metallurgical Quarterly · 2009 · 23 citations · 11 references

Concepts

Abstract

AbstractMagnesium alloy AE42 has long been recognized as a superior high temperature magnesium alloy for aerospace and automotive components. The elevated temperature strength of this alloy is attributed to the Mg-Alx-REy intermetallics on the grain boundaries preventing grain boundary sliding. However, these intermetallics also hinder interdendritic liquid feeding during casting solidification and contribute to the alloy's high susceptibility to hot tearing.In this research, the conditions associated with the onset of hot tearing in the AE42 alloy were identified. Thermal analysis suggested that a casting with a hot tear experienced long vulnerable interval, when interdendritic feeding was minimal and the alloy was susceptible to hot tearing. Microscopic analysis revealed the presence of interdendritic shrinkage pores with Al-RE intermetallics at hot-tear nucleation sites. Further, the elastic residual strain measured by neutron diffraction indicates that tensile strain resulting from contraction of the casting during solidification was responsible for opening and propagation of hot tears in the AE42 alloy.Magnesium alloy AE42 has long been recognized as a superior high temperature magnesium alloy for aerospace and automotive components. The elevated temperature strength of this alloy is attributed to the Mg-Alx-REy intermetallics on the grain boundaries preventing grain boundary sliding. However, these intermetallics also hinder interdendritic liquid feeding during casting solidification and contribute to the alloy's high susceptibility to hot tearing.In this research, the conditions associated with the onset of hot tearing in the AE42 alloy were identified. Thermal analysis suggested that a casting with a hot tear experienced long vulnerable interval, when interdendritic feeding was minimal and the alloy was susceptible to hot tearing. Microscopic analysis revealed the presence of interdendritic shrinkage pores with Al-RE intermetallics at hot-tear nucleation sites. Further, the elastic residual strain measured by neutron diffraction indicates that tensile strain resulting from contraction of the casting during solidification was responsible for opening and propagation of hot tears in the AE42 alloy.On a reconnu depuis longtemps que l'alliage de magnésium AE42 était un alliage de magnésium supérieur pour température élevée des composantes aérospatiales et automobiles. La résistance à haute température de cet alliage est attribuée aux composés intermétalliques Mg-Alx-REy aux joints de grain empêchant le glissement des joints de grain. Cependant, ces composés intermétalliques empêchent également l'alimentation de liquide interdendritique lors de la solidification de moulage et contribuent à la susceptibilité élevée de l'alliage à la fissuration à chaud.Dans cette recherche, on a identifié les conditions associées au début de la fissuration à chaud de l'alliage AE42. L'analyse thermique suggère qu'un moulage avec fissure à chaud a eu pour expérience un long intervalle de vulnérabilité lorsque l'alimentation interdendritique était minimale et que l'alliage était susceptible à la fissuration à chaud. L'analyse microscopique a révélé la présence de pores de retassure interdendritique avec des composés intermétalliques Al-RE aux sites de nucléation de fissure à chaud. De plus, la déformation élastique résiduelle mesurée par diffraction des neutrons indique que la résistance à la traction résultant de la contraction du moulage lors de la solidification était responsable de l'ouverture et de la propagation de fissures à chaud de l'alliage AE42.

References

11