The pH-dependent transformation of schwertmannite to goethite at 25°C

U. Schwertmann, L. Carlson

Clay Minerals · 2005 · 135 citations · 9 references

Concepts

Abstract

Abstract At 25°C, synthetic schwertmannite, a common iron compound in acid mine drainage, completely converted in water to a sulphate-containing goethite within ~100 days. The rate of transformation doubled as the pH increased from 4.0 to 7.2. In deviation from its normal acicular habit, the goethite appeared as spherical aggregates.

References

9