Powder Metallurgy · 1995 · 18 citations · 16 references
Natural SciencesMaterials EngineeringMaterials ScienceCorrosion ScienceImplant SurgeryMetallurgyAlloysCorrosion EngineeringCorrosion ResistanceCorrosion-resistant MaterialsImplant MaterialsSinteringCobalt-chromium AlloysCorrosion Resistance MaterialsCorrosion-resistant AlloysPore GeometryPore Geometry EffectsPore Size EffectsPorous Implant MaterialsSurgical Implant Placement
In the first part of this study, data were presented for the compaction, sintering, and mechanical properties of a water atomised cobalt based alloy and a bimodal mixture of ball milled ASTM F75 plasma rotating electrode process powder blended with the cobalt based alloy powder. In the present study, the corrosion of these two powders was compared for a range of compacts of varying porosity between 6 and 35% total porosity and between 0·5 and 26% interconnected porosity under conditions which simulated in vitro body fluid conditions. Differences in microstructure and surface composition caused by reactions with three different sintering atmospheres, e.g. loss of chromium, decarburisation, or Cr 2 N formation, altered the corrosion behaviour. The worst corrosion resistance occurred in compacts sintered in molecular 75H 2 –25N 2 (by volume) gas, while argon atmosphere sintered compacts were the most resistant to corrosion. Pore size and pore geometry also had a considerable influence on the corrosion behaviour and the corrosion resistance tended to improve with decreasing porosity. PM/0694
16