Journal of the American Ceramic Society · 1977 · 131 citations · 10 references
Natural SciencesMaterials EngineeringMaterials ScienceAnalytical ChemistryInorganic ChemistryPhysical ChemistryPeritectic TransformationsPhase AnalysisPhase DiagramsPhase EquilibriaPhase RelationsSolution ChemistryChemical EquilibrationEutectic Melting TemperatureMelting TemperatureOxygen SolubilityPeritectic Phase DiagramSolubilitySolubility BehaviorSolubility Limits
The melting, eutectic, peritectic, solidus, and liquidus temperatures in the system Zr‐O have been measured directly by a simple optical pyrometric technique requiring only a few hundred milligrams of sample. The saturation solubility of oxygen in α‐Zr( s ) between 1270° and 1980°C and the lower phase boundary of the ZrO 2 – α phase between 1900° and 2400°C have been measured by an isopiestic equilibration method. The oxygen solubility limit in α‐Zr( s ) agrees well with previous low‐temperature studies and reaches a maximum solubility of 35°1 at.% O at the eutectic temperature, 2065°°5°C. The maximum melting temperature of α‐Zr( ss ) is 2130°°10°C and corresponds to a composition of 25°1 at.% O. Both of these temperatures are approximately 150° higher than previously reported. Liquidus compositions above the eutectic temperature were obtained via mass spectrometry from the kinetic behavior of the liquid solution‐ZrO 2–x ( s ) mixture as it approached equilibrium at 2125°°5°C. The lower phase boundary or solidus of the ZrO 2–x phase departs appreciably from ideal stoichiometry above 1900°C and smoothly reaches its most reduced composition, 61 at.% (ZrO 1.56 ), near 2300°C. The solidus is retrograde at higher temperatures. The melting temperature of the stoichiometric dioxide is 2710°°15°C.
10
Max Hansen, K. Anderko, H. W. Salzberg · Journal of The Electrochemical Society · 1958 · 14.8K citations