Magnetic Properties of Nickel–Zinc Ferrite Toroids Prepared from Nanoparticles

Brian Naughton, David R. Clarke

Journal of the American Ceramic Society · 2007 · 32 citations · 13 references

Concepts

Abstract

Toroids comprised of silica‐coated 10 nm diameter nickel–zinc (Ni–Fe) ferrite nanoparticles (Ni 0.5 Zn 0.5 Fe 2 O 4 ) have been fabricated by careful control of both the coating process and subsequent densification by viscous sintering. A narrow processing window is identified between a maximum temperature at which the nanoparticles coarsen, losing their super‐paramagnetic properties, and a lower temperature required for viscous flow densification. Key to the successful fabrication was drying and cold isostatic pressing of the silica‐coated nanoparticles; other routes invariably led to cracking during either drying or sintering. The super‐paramagnetic blocking temperature, the coercive field, and remanent magnetization could all be controlled over a wide range by varying the thickness of the silica coating from 1 to 15 nm. The dipole–dipole coupling distance is estimated to be 4 nm. The high‐frequency (1–500 MHz) properties were sensitive to the sintering temperature as well as the thickness of the silica coating. Toroids sintered at 1000°C or less exhibited no high‐frequency magnetic losses and their permeability decreased with increasing temperature, suggesting that the permeability was controlled by thermally activated magnetization relaxation.

References

13