High Temperature Deformation Mechanism of a High-Purity Fe–50 mass% Cr Alloy

S. Isozaki, S. Takaki, K. Abiko

physica status solidi (a) · 1998 · 13 citations · 4 references

Concepts

Abstract

The deformation mechanism of a high-purity Fe–50 mass% Cr alloy and a floating-zone refined Fe–50 mass% Cr alloy was investigated by tensile testing between 873 and 1073 K and microstructural observation. It is concluded from the present experimental research that: 1. A stress-drop appears after yielding in both alloys between 873 and 1073 K. The stress-drop is the result of grain boundary sliding and is related to the formation of dislocation sources at the beginning of deformation. 2. Intergranular cracking occurs in the high-purity Fe–50 mass% Cr alloy and also in the fine-grained zone-refined alloy and the cracking is strongly influenced by grain size. The mechanism is not grain boundary decohesion caused by segregated sulfur. 3. The stress-drop is also observed in the Fe–50 mass% Cr–8 mass% W alloy, but grain boundary cracks are seldom observed in this alloy. 4. The deformation behavior after the stress-drop is determined by a competition between increasing dislocation density and dislocation annihilation at high temperatures. No twinning is seen in this temperature range, not even in the W-doped alloy.

References

4