Investigation of cracks and sensitization in an AISI 304L stainless steel exposed to 500–600°C

V. Moura, Y.A. Kina, Sérgio Souto Maior Tavares, M.M.S.G. de Faria, Fernando B. Mainier

Engineering Failure Analysis · 2008 · 19 citations · 4 references