DentistryDental Materials ScienceCeramic MaterialsCeramicsDental MaterialsCementitious MaterialsComposite ResinsDegradation Of Dental MaterialsDental CeramicsDental CompositesBiodegradation Of Dental CompositesCrack FormationDegradation Of Dental CeramicsDental Composite FillersHydrolytic Degradation AnalysisHydrolytic Degradation StudiesMatrix-filler InterfacesOsmotic Pressure
This study evaluated the hydrolytic degradation of two experimental (C1, C2) and two commercial composite (Tetric EvoCeram and Premise) prepared to be used in dental restorations. Two experimental composites and two commercial composites were undergoing hydrolytic degradation in three different medium: distilled water, artificial saliva and alcoholic solution (50/50). The samples were investigated immediately after polymerisation with halogen lamp Optilux 501 and after 33 days of immersion in all three medium, using Fourier transforms infrared analysis (FTIR). FT-IR spectra of samples from the same composite immersed in distilled water, artificial saliva and alcoholic solution, revealed mostly reducing the intensity of the characteristic peaks of Si-O-Si bond less Tetric composite immersed in artificial saliva, which peak intensity remains unchanged.
10
Hydrolytic Degradation of Dental Composites
K.-J.M. Söderholm, M. Zigan, M. Ragan et al. · Journal of Dental Research · 1984 · 535 citations