Critical behavior of the electrical resistance of very thin Cr films

J. A. J. Lourens, Sigurds Arajs, H. F. Helbig, E. A. Mehanna, L. Cheriet

Physical review. B, Condensed matter · 1988 · 24 citations · 8 references

Concepts

Abstract

Measurements of the thickness dependence of the electrical resistance of two very thin Cr films deposited at substrate temperatures of 385 and 360 \ifmmode^\circ\else\textdegree\fi{}C and pressures of ${10}^{\mathrm{\ensuremath{-}}7}$ and ${10}^{\mathrm{\ensuremath{-}}6}$ Torr are reported. The various conduction mechanisms have been identified and a metal-insulator region spanning about 5.5 nm of thickness has been found. In this region the resistance of both films follows the scaling law R\ensuremath{\propto}(d-${d}_{c}$${)}^{\mathrm{\ensuremath{-}}t}$ with t=1.34\ifmmode\pm\else\textpm\fi{}0.11 and ${d}_{c}$ equal to 1.64\ifmmode\pm\else\textpm\fi{}0.20 and 1.03\ifmmode\pm\else\textpm\fi{}0.20 nm.

References

8