Journal of Materials Chemistry · 1997 · 97 citations · 21 references
Natural SciencesMaterials EngineeringMaterials ScienceCeramic MaterialsInorganic ChemistryMaterials ChemistryPowder ProcessingSinteringThermal Properties Of CeramicsCombustion SynthesisElectrical Conductivity MeasurementsLanthanide OxidesManganese OxidesManganitesRhombohedral Unit CellsSurface AreaThermal Expansion
Strontium substituted lanthanum manganites La1–xSrxMnO3 (x=0, 0.1, 0.16, 0.2 and 0.3) have been prepared by a solution combustion process using lanthanum nitrate, strontium nitrate and manganese nitrate as oxidizers and oxalyl dihydrazide as fuel at 300 °C in a pre-heated muffle furnace. As-formed lanthanum manganites are X-ray crystalline showing cubic symmetry. The cubic LaMnO3 with 36% Mn4+ changes to a rhombohedral phase (Mn4+=28%) on calcination at 1000 °C. The surface area and average agglomerated particle size of the as-formed manganites are in the range 12–19 m2 g–1 and 5.4–8.0 µm, respectively. Sintering, thermal expansion and dc electrical conductivity measurements of La(Sr)MnO3 have been carried out. Strontium substituted lanthanum manganites achieve >80% theoretical density after sintering at 1350 °C for 4 h and the percentage theoretical density decreases with increasing strontium content. The thermal expansion coefficient of La(Sr)MnO3 increases with increasing Sr2+ content and La0.84Sr0.16MnO3 shows a highest conductivity value of 202 S cm–1 at 900 °C in air.
21
Nguyen Q. Minh · Journal of the American Ceramic Society · 1993 · 3.8K citations
Natural Sciences, Materials Engineering, Materials Science +17
B.C. Tofield, Walter R. P. Scott · Journal of Solid State Chemistry · 1974 · 403 citations
Natural Sciences, Materials Engineering, Materials Science +15