Relaxation of shish‐kebab precursor in isotactic polystyrene after short‐term shear flow

Yunfeng Zhao, Go Matsuba, Koji Nishida, Tetsuaki Fujiwara, Rintaro Inoue, Inga A. Polec, Cong Deng, Toshiji Kanaya

Journal of Polymer Science Part B Polymer Physics · 2010 · 22 citations · 27 references

Concepts

Abstract

Abstract We studied the formation and relaxation of precursors of shish‐kebab in isotactic polystyrene after applying pulse shear flow at temperatures above the nominal melting temperatures T m (=223 °C). It was found that the string‐like objects that were assigned to precursors in a previous article appeared in micrometer scale up to ∼285 °C, which was very close to the equilibrium melting temperature T (=289 °C), and the length and the diameter showed two‐step decays consisting of the fast and slow (almost nondecaying) components below ∼270 °C, whereas the slow component disappeared above ∼270 °C, suggesting that some mechanism stabilizing the string‐like objects disappeared at ∼270 °C. It was also found that the two‐step decay was a nature of a single string‐like object, but not an average nature of many precursors, showing heterogeneous inner structure of the precursor. We discussed a possibility that the string‐like object had a fringed micelle type structure including large crystals with a melting temperature of ∼270 °C. Within the proposed picture, the highest temperature for the precursor formation (∼285 °C) was explained as a melting of the large crystals in oriented melt. © 2010 Wiley Periodicals, Inc. J Polym Sci Part B: Polym Phys, 2010

References

27