Electrodeposition of Molydenum Alloys from Aqueous Solutions

D. W. Ernst, R. F. Amlie, M. L. Holt

Journal of The Electrochemical Society · 1955 · 59 citations · 0 references

Concepts

Abstract

Nickel-molybdenum, cobalt-molybdenum, and iron-molybdenum alloys have been electrodeposited, from aqueous olutions containing sodium molybdate, the sulfate of the codeposited metal, sodium citrate, and ammonium hydroxide. Typical baths were made up with 0.3 M/1 of the codepositing metal sulfate, 0.3 M/1 of sodium citrate, vary-ing amounts of sodium molybdate, and ammonium hydroxide to pH about 10.5. The maximum amount of molybdenum in the electrodeposited alloys depends on the alloying metal. When a typical bath was used, nickel alloys were found to contain up to 20% molybdenum, cobalt al oys contained up to 40 % molybdenum, and iron alloys contained about 50 % molybdenum. The cathode current efficiency in the above cases ranged from 75-85 % for the nickel-molybdenum bath, 50-60 % for cobalt-molybdenum, and 10-20% for iron-molybdenum. The effects of pH, concentration, temperature, and cathode cur-rent density on cathode current efficiency and alloy composition were studied. These electrodeposited molybdenum alloys were metallic and either bright or light gray in appearance, with a large number of cracks in the bright deposits. Adherence of the deposit o well-cleaned flat cathodes eemed to be good, but adherence to tubing or rods was poor; usually these deposits could be brushed off in flake or powder form.