The hydration of tricalcium and β‐dicalcium silicates in pastes under normal and steam curing conditions

E. R. Buckle, H. F. W. Taylor

Journal of Applied Chemistry · 1959 · 22 citations · 13 references

Concepts

Abstract

Abstract Pastes of tricalcium silicate (C 3 S)* and β‐dicalcium silicate (β‐C 2 S) have been cured at various temperatures mainly in the range 18–200°. Over the whole of this range, C 3 S reacts more quickly than β‐C 2 S, giving initially a matrix composed of very badly crystallised material related to tobermorite, mixed with Ca(OH) 2 . With C 3 S at about 50° and above, other compounds are also formed, crystallising usually, if not always, from this matrix, and replacing it completely at the higher temperatures. C 2 α‐hydrate is thus formed at 130–200°, and C 3 H 1.5 in two distinct ranges, 50–170° and 190–500°. Above 300°, calcio‐chondrodite (C 2.5 SH 0.5 ) is also formed. With β‐C 2 S pastes at all temperatures below 200° the initial product is similarly a matrix of tobermoritic material, but little or no C a (OH) 2 is formed. C 2 α‐hydrate crystallises from this matrix at 120–180°, but no C 3 SH 1.5 is formed. Dehydration isobars afforded tentative quantitative phase analyses for several cured pastes. The Ca/Si ratio estimated for the tobermoritic material in C 3 S pastes cured at room temperature is about 1.7.

References

13