Transport Coefficients of Oligo- and Poly(α-methylstyrene)s in Dilute Solution

Ikuko Suda, Yumiko Tominaga, Masashi Osa, Takenao Yoshizaki, Hiromi Yamakawa

Macromolecules · 2000 · 13 citations · 27 references

Concepts

Abstract

The intrinsic viscosity [η] was determined for 25 samples of atactic oligo- and poly(α-methylstyrene)s (a-PαMS), each with the fraction of racemic diads f r = 0.72, in the range of weight-average molecular weight M w from 2.94 × 10 2 (dimer) to 3.22 × 10 6 in cyclohexane at 30.5 °C (ϑ). The translational diffusion coefficient D was also determined from dynamic light-scattering measurements for 21 of them in the range of M w from 5.30 × 10 2 (tetramer) to 3.22 × 10 6 under the same solvent condition. It is found that the double-logarithmic plots of [η] and M w D against M w follow their respective asymptotic straight lines of slope 1 / 2 for M w ≳ 2 × 10 5, but deviate upward and downward, respectively, from them with decreasing M w for smaller M w . From an analysis of these transport coefficients on the basis of the helical wormlike (HW) chain model, it is shown that the above M w dependence of [η] and D may be well explained by the corresponding HW theories with the values of the model parameters consistent with those previously determined from the mean-square radius of gyration 〈 S 2 〉. A comparison is also made of the present results for [η] and D for a-PαMS with the previous ones for atactic polystyrene with f r = 0.59, atactic poly(methyl methacrylate) (a-PMMA) with f r = 0.79, and isotactic PMMA with f r ≃ 0.01. It confirms the previous conclusion derived from 〈 S 2 〉 concerning the chain stiffness and local chain conformations of the a-PαMS chain. That is, the a-PαMS chain tends to retain large and clearly distinguishable helical portions in dilute solution just as the a-PMMA chain, although the strength of helical nature is somewhat smaller for the former.

References

27