The corrosion behavior of several heat resistant materials in air + 2% Cl2 at 300 to 800 °C. Part 3 - Alumina formers and intermetallics

C. Schwalm, M. Schütze

Materials and Corrosion · 2000 · 17 citations · 0 references

Concepts

Abstract

The corrosion behavior of Alloy 214 and the intermetallics Fe3Al, TiAl and MoSi2 was investigated in dry air and air with 2% Cl2 at temperatures of 300 to 800 °C. The results show that corrosion resistance of Alloy 214 and the two aluminides very much depend on the test temperature. For TiAl massive corrosion starts at 500 °C. Alloy 214 shows corrosion rates similar to chromia formers at temperatures of 650 and 800 °C while the best corrosion resistance of all alumina formers tested is revealed by Fe3Al. For MoSi2 only some little (“internal”) oxidation is observed even at 800 °C.