Journal of Environmental Engineering · 2000 · 20 citations · 14 references
EngineeringMaterials EngineeringMaterials ScienceConstruction MaterialsSolid Waste ManagementWaste ManagementIron OxidesWaste DisposalWaste Form DevelopmentWaste TreatmentArsenic ChemistryHeavy Metal StabilizationInorganic SaltsLeachingMole RatiosWaste Form Stabilization
Effective solidification/stabilization (S/S) of arsenic- and barium-containing D004/D005 waste was accomplished by using a binder of cement with 40% class C fly ash and either ferrous sulfate or ferric sulfate as an additive. Addition of iron salts improves arsenic solidification/stabilization (S/S). Barium may be encapsulated within the stabilized matrix as barium sulfate. Recommended mole ratios for iron/arsenic and barium/sulfate are at least 6 and 1.2, respectively. A binder/waste ratio of 0.15 is volume efficient, but the mix design must be carefully controlled to achieve adequate S/S. In practice, the heterogeneity of waste and large-scale mix operations may preclude close control of reagent dosages, so a binder/waste ratio of 0.40 is preferable. Ferrous sulfate additive is preferable for arsenic S/S because it is effective over a wider range of mix designs and over a long-term curing period. Toxicity characteristic leaching procedure results degraded with long curing time for some mix designs with ferric sulfate additive.
14