Superconductor Science and Technology · 2006 · 53 citations · 8 references
Natural SciencesElectrical EngineeringMaterials ScienceElectromagnetismElectronic MaterialsThin FilmsElectrical ConductivityHigh-temperature MaterialsStrain EngineeringSuperconducting MaterialsThin Film Electrical PropertiesThin Film StrainCritical Current DensityCritical Current PerformanceCurrentsElectric Field EffectsStrain Effects On Electronic PropertiesSuperconducting TapesTemperature Dependence Of I-v Curves
The strain dependence of the critical current in Y-123 tapes has been studied as a function of field and temperature up to strain values of 0.81%. For the particular tape configuration with a Ni–W substrate, the critical current was found to be reversible up to 0.51%. The Ic(ε) curves have been measured at 4.2, 50 and 77 K at fields up to 19 T. In the reversible region, the decrease of Ic(ε)/Ic(ε = 0) with ε was found to be more pronounced at higher fields and temperatures: at 17 T the decrease of Ic/Ico at εirr was of the order of 9% and 25% at 4.2 and 50 K, respectively. At 77 K and 6 T, the corresponding decrease was 12%. Using the Walters spiral for tapes up to 0.80 m length, the V –I curves have been measured over three decades. At low electric field (0.01 µV cm−1) the n value is constant up to 0.81% strain, while at higher electric field it decreases with the applied strain.
8