Macromolecules · 2012 · 38 citations · 37 references
Natural SciencesMaterials EngineeringMaterials SciencePolymer ChemistryPolymer EngineeringPolymer MaterialsFiber PropertiesPolymer CharacterizationPolymer PhysicsElectrospinningFibersPolyethylene TerephthalateRheological CharacterizationSmall-angle X-ray ScatteringViscosityWide-angle X-ray ScatteringZero-shear Viscosity
Electrospun poly(ethylene terephthalate) (PET) fibers were prepared from a trifluoroacetic acid (TFA)-based solvent. Rheological studies revealed the concentration (ϕ) dependence of the specific viscosity (η sp ) to be η sp ∼ ϕ 3.7 for PET/TFA solutions in the entangled regime. The determined entanglement concentration (ϕ e ) was higher using a lower-molecular-weight PET. To obtain bead-free fibers, the minimum concentration for the electrospinning was 0.8–1.0ϕ e owing to the high volatility of TFA solvent, which significantly enhanced the chain network strength during jet whipping. The double-logarithmic plots of the jet ( d j ) and fiber ( d f ) diameters versus the zero-shear viscosity (η 0 ) revealed that two scaling laws existed for the present solutions, i.e., d j ∼ η 0 0.06 and d f ∼ η 0 0.77 . The microstructural evolution of the electrospun PET fibers from stepwise annealing to crystal melting was investigated by simultaneous small-angle X-ray scattering (SAXS)/wide-angle X-ray diffraction (WAXD) measurements using synchrotron radiation sources. The conformer transformation from gauche to trans was monitored by in-situ Fourier transform infrared spectral measurement. In the absence of any WAXD reflection, the as-spun PET fibers possessed a SAXS scattering peak, indicating the presence of a mesomorphic phase with an interdomain distance of 6.8 nm. At annealing temperatures ( T a ) higher than 100 °C, the mesomorphic phase gradually transformed into imperfect triclinic crystals and reached its saturation at 130 °C. Further increased T a perfected the triclinic structure without altering fiber crystallinity until the initial crystal melting at 218 °C, at which a significantly increased long period was detected. When the electrospun PET fibers were embedded in an isotactic polypropylene (iPP) matrix, surface-induced crystallization occurred to develop a transcrsytalline layer of iPP monoclinic crystals at the interface.
37
Electrospinning of polyurethane fibers
Mustafa M. Demir, Burak Erman · Polymer · 2002 · 1.1K citations
Natural Sciences, Materials Engineering, Materials Science +9
Pankaj Gupta, Casey L. Elkins, Timothy E. Long et al. · Polymer · 2005 · 826 citations
Natural Sciences, Materials Engineering, Materials Science +14