Materials and Corrosion · 2000 · 19 citations · 0 references
Natural SciencesMaterials EngineeringMaterials ScienceCorrosion ScienceMetallic MaterialsMetallurgyCorrosion EngineeringCorrosion MechanismsCorrosion TestingFracture MechanicsStainless SteelsStress Corrosion CrackingAustenitic Stainless SteelsCrack GrowthCrack Growth TestingStainless Steel CorrosionStress Corrosion Cracking TestingThreshold Stress IntensityTransgranular Stress Corrosion CrackingWeld Testing
Compact tension specimens of nitrogen-added AISI type 316 austenitic stainless steel and its weld metal were subjected to stress corrosion cracking (SCC) testing in a boiling solution containing 5 M sodium chloride + 0.15 M sodium sulphate + 2.5 ml/l hydrochloric acid solution using the constant extension rate testing (CERT) technique. The extension rate of testing was 10 microns per hour. The threshold values of stress intensity factor (KISCC) and J-integral (JISCC) were taken as those values of KI and JI at which about 25 microns of SCC crack growth was observed. These threshold values were about four times higher and plateau crack growth rates (PCGR) were nearly one order of magnitude lower for the base metal vis-à-vis the weld metal. Fractographic observations indicated failure by transgranular SCC (TGSCC) of austenite in both the base and weld metal. No stress-assisted dissolution of delta-ferrite or its interface with austenite, was observed.