Journal of Esthetic and Restorative Dentistry · 2001 · 12 citations · 2 references
DentistryDental Materials ScienceRestorative DentistryDental MaterialsMechanical Properties Of Dental MaterialsPolymerization Of Dental ResinsComposite Resin RestorationsComposite ResinsDental CompositesDentin BondingEnamel Mechanical PropertiesEnamel-dentin JunctionDentin Bonding AgentsElastic Modulus DevelopmentFlexural StrengthFlexural Strength DevelopmentLight-cured Dental ResinsLight-curing EffectsPolymerization Light Exposure
ABSTRACT Objective : This in vitro study examined the effect of light intensity variations on several properties of two restorative systems. Materials and Methods : Two resin composite systems (Tetric, Ivoclar Vivadent, Schaan, Liechtenstein; 2100, 3M Dental Products Division, St. Paul, Minnesota) and two dentin bonding agents (Syntac, Ivoclar Vivadent; Scotchbond Multi‐Purpose, 3M Dental) were used. To evaluate marginal gap formation in dentin cavities (with a C factor of 2.5), 48 bovine incisors were embedded in epoxy resin. The labial enamel was removed, and the dentin surface was polished to 600‐grit. Preparations were made in dentin and restored using one of four combinations of bonding system and composite. The composite was polymerized with either a high‐intensity lamp (450 mW/cm 2 ) or a low‐intensity lamp (250 mW/cm 2 ). After storage in water for approximately 60 minutes, the surfaces of the samples were prepared for electron microscopy analysis. Also, the flexural strength and modulus of each composite were determined at 30 minutes and 24 hours after polymerization with either the high‐ or low‐intensity light. Volumetric shrinkage was measured using the density method at four time periods for both light intensities and for wet versus dry storage. Finally, Vickers hardness profiles were evaluated to determine depth of cure. Results : Marginal analysis showed that 2100, when used with either Scotch‐bond Multi‐Purpose or Syntac, had an increased incidence of gap formation when polymerized with the high‐intensity light. Tetric had better marginal adaptation than 2100, when used with either dentin bonding agent, and with both light intensities. The flexural strength and modulus of both composites were lower with low‐intensity light‐curing. There were no differences in volumetric shrinkage or depth of cure related to curing method for either composite. Conclusions : The results of this study suggest that marginal quality may be reduced when a high‐intensity light is used to cure composite. Also, the light intensity influences development of the elastic modulus and, therefore, affects shrinkage stress in the composite. The two composites tested in this study responded differently to the different methods of light‐curing. In general, Z100 showed inferior properties than Tetric when cured with either high‐ or low‐intensity light, for both marginal integrity and the flexural modulus and strength. Finally, with a polymerization time of 40 seconds, the composites were equally well cured to a depth of 4.5 mm, regardless of the light intensity used.
2