Entrapped Gas Effect in the Fast Firing of Yttria‐Doped Zirconia

Do‐Hyeong Kim, Chong Hee Kim

Journal of the American Ceramic Society · 1992 · 31 citations · 5 references

Concepts

Abstract

Compared to conventional sintering of Y 2 O 3 ‐doped ZrO 2 using a slow heating rate of 10°C/min, microwave sintering and fast firing using a rapid heating rate of about 500°C/min resulted in lower final sintered densities. It is attributed to the residual chlorine in commerical zirconia powders manufactured by the chloride process. By calcining at 1100°C for 1 h to remove residual chlorines from the powder compacts, near full densities (>99% of theoretical) could be obtained by both fast firing and microwave sintering.

References

5