Journal of The Electrochemical Society · 1975 · 54 citations · 0 references
Natural SciencesMaterials EngineeringMaterials ScienceCorrosion ScienceElectrochemistryMetallic MaterialsCorrosion EngineeringCorrosion KineticsCorrosion MechanismsCorrosion-resistant MaterialsElectrochemical CorrosionAnodic DissolutionCrackingCurrent DensityElectrochemical Corrosion ProcessesElectrochemical MechanismsElectrolyte Concentration EffectsPassive FilmPassive Film Formation
Repassivation current transients in the Fe-caustic system were measured after straining potentiostatically polarized electrodes with a drop weight apparatus, which could produce strains of about 5 % in 1 msec. Peak current densities varied from 0.3 to 3.8 A/cm " depending on electrode potential, elec-trolyte concentration, and temperature, and initial film coverage was com-plete in less than 1 or 2 msec. The amount of corrosion accompanying passive film formation was not very sensitive to the above-mentioned electro-chemical variables, and it ranged from 1 • 10-3 to 5 X 10-3 coulombs/cme. Repassivation was facilitated by additions to the test electrolyte of the anodic dissolution product HFeO2-. The total corrosion up to 1 sec following straining was a strong function of potential, electrolyte concentration, and temperature, as was the quasi steady-state current density. The depth of corrosion 1 sec after straining ranged from twenty to several hundred angstrom units. The relevance of these results to several mechanistic models of caustic cracking is