Study of the Thermal Stability and Mechanical Characteristics of MAX Phases of Ti-Al-C(N) System and their Solid Solutions

T. A. Prikhna, Thierry Cabioc’h, W. Gawalek, D. Litzkendorf, M. G. Loshak, V. B. Sverdun, Patrick Chartier, Tetyana Basyuk, Viktor Moshchil, Artem Kozyrev,

Advances in science and technology · 2014 · 10 citations · 10 references

DOIFull text

Open access

Concepts

Abstract

The DTA and TG study in air of Ti 2 Al (C 1-x N x ) and Ti 3 AlC 2 synthesized under Ar 0.1 MPa pressure and densified in thermobaric conditions at 2 GPa, 1400 °C, for 1 h showed that the increase of the amount of TiC layers in Ti-Al-C MAX phases structures leads to the increase of their stability against oxidation: 321 MAX phase Ti 3 AlC 2 are more stable than Ti 2 AlC and Ti 2 Al (C 1-x N x ) solid solutions both before and after thermobaric treatment. The oxide film formed on the surface of the highly dense (ρ=4.27 g/cm 3 , porosity 1 %) material based on nanolaminated MAX phase Ti 3 AlC 2 (89 % Ti 3 AlC2, 6 % TiC, 5 % Al 2 O 3 ) manufactured by hot pressing (at 30 MPa) made the material highly resistant in air at high temperatures: after 1000 hours of exposition at 600 °C it demonstrated a higher resistance to oxidation than chromium ferrite steels (Crofer GPU and JDA types). Due to the surface oxidation self-healing of defects took place. Besides, the Ti 3 AlC 2 material demonstrated resistance against high-temperature creep and after being kept in H 2 at 600 °C for 3h its bending strength reduced by 5 % only. At room temperature the Ti 3 AlC 2 bulk exhibited microhardness Hμ = 4.6 GPa (at 5 N), hardness HV 50 = 630 (at 50 N ) and HRA = 70 (at 600 N), Young modulus was 140 ± 29 GPa, bending strength =500 MPa, compression strength 700 MPa, and fracture toughness K 1C =10.2 MPa·m 0.5 .

References

10