Prevention of Nanoparticle Coalescence under High-Temperature Annealing
61
Citations
29
References
2004
Year
Materials ScienceNanoparticlesNano ApplicationHigh-temperature AnnealingEngineeringMagnetic Data StorageNanomaterialsNanotechnologySerious CoalescenceNanoscale ChemistryApplied PhysicsNanostructure SynthesisSio2 SubstrateChemistryFept NanoparticleNanocrystalline MaterialMagnetic Medium
An effective method of employing 3-aminopropyldimethylethoxysilane linker molecules to stabilize 4.4 nm FePt nanoparticle monolayer films on a SiO2 substrate as well as to prevent coalescence of the particles under 800 degrees C annealing is reported. As-deposited FePt nanoparticle films in chemically disordered face-centered-cubic phase transform to mostly chemically ordered L1 0 structure after annealing, while the nanoparticles are free from serious coalescence. The method may fulfill the pressing need to prevent nanoparticle coalescence under high-temperature annealing for the development of FePt nanoparticle based products, such as ultrahigh-density magnetic recording media and novel memory devices.
| Year | Citations | |
|---|---|---|
Page 1
Page 1