Oxidation Kinetics and Composite Scale Formation in the System Mo(Al,Si) <sub>2</sub>

C. Eric Ramberg, W. L. Worrell

Journal of the American Ceramic Society · 2002 · 37 citations · 26 references

Concepts

Abstract

The oxidation kinetics of hot‐pressed Mo(Al 0.01 Si 0.99 ) 2 and Mo(Al 0.1 Si 0.9 ) 2 were measured at 480°C, and between 1200° and 1600°C. The qualitative oxidation of arc‐melted Mo(Al 0.1 Si 0.9 ) 2 , Mo(Al 0.3 Si 0.7 ) 2 , Mo(Al 0.5 Si 0.5 ) 2 , and Mo 3 Al 8 was examined after 600°C for 1000 h in air. At all temperatures, the compositional difference between the materials yielded very different oxidation rates and scale microstructures. At 1400° and 1500°C, microstructural evolution of the oxide scales resulted in improved oxidation resistance at long times (&gt;400 h). At these temperatures, a significant reduction in the long‐time oxidation kinetics was correlated with the in situ formation of an inner mullite scale. At 480° and 600°C, oxidation resistance improved significantly with increasing aluminum concentration. Contrary to the behavior of MoSi 2 , samples of Mo(Al 0.01 Si 0.99 ) 2 did not demonstrate catastrophic oxidation, and samples of Mo(Al 0.1 Si 0.9 ) 2 were very oxidation resistant.

References

26