Oxidation Properties of (U, Pu)O2 Solid Solutions

V.J. Tennery, T.G. Godfrey

Journal of the American Ceramic Society · 1973 · 27 citations · 8 references

Concepts

Abstract

Air oxidation of (U, Pu)O 2 solid solutions having Pu/(U+Pu) ratios of 0.2 and 0.25 was studied using a recording thermal balance. For Pu/(U+Pu)=0.2, the original fluorite MO 2 phase oxidized first to tetragonal M 3 O 7 ; further oxidation at 450°C< T <600°C gave a two‐phase mixture of M' 3 O 8 and a cubic phase having a 0 ≃5.43 Å. Kinetic analysis of these oxidation stages indicated that the Erofeev nucleation model explains the data reasonably well, with Δ H ≃40 kcal/mol for the formation of M 3 O 7 and Δ H ≃40 kcal/mol for the oxidation of M 3 O 7 to M' 3 O 8 + the cubic phase. Oxidation above M 3 O 7 (O/M=2.35) resulted in mechanical disintegration of the samples because of the presence of the M' 3 O 8 phase. For Pu/(U+Pu) = 0.25, both isothermal and programed air oxidation of homogeneous samples up to 800°C led to a compound with a maximum O/M≃2.35, i.e. M 4 O 9.4 , an fcc phase having a 0 =5.428 Å; these samples were not converted to powder by the oxidation.

References

8