Abstract

Abstract Indium tin oxide (ITO) whiskers were grown by VLS (vapour‐liquid‐solid) mechanism, using the electron shower method. The whiskers were grown above 200 °C, and the deposition rate was above 0.6 nm/s. The electron shower controlled the size of the whiskers, and the size was 30 nm in diameter and 600 nm in length. The whiskers grew along the substrate at t < 300 s, but grew in a direction perpendicular to the substrate at t > 300 s. When the ITO whiskers grown along the substrate were used as NO 2 gas sensor, the sensitivity was 340, and about 300 times higher than those of the whiskers grown in a direction perpendicular to the substrate and plate‐like ITO crystallites.