Influence of Prior Deformation and Composition on Continuous Cooling Sensitization of AISI 304 Stainless Steel

H. D. Solomon

CORROSION · 1985 · 15 citations · 5 references

Concepts

Abstract

This paper addresses the question of the combined effect of carbon content and prior cold work on the sensitization of AISI 304 stainless steel (SS). It was found that prior cold work increased the critical cooling rate required to produce sensitization (i.e., made it easier) for steels containing from 0.017 to 0.077 wt% C. Both A262 practice A and practice E tests were used. The A262A test revealed sensitization at higher cooling rates than the A262E test (for all heats studied). The influence of peak temperature was also studied. Sensitization was found to be most rapid when the peak temperature was in the 700 to 800 C range, with the exact temperature depending upon the carbon content.

References

5