Journal of the American Ceramic Society · 1997 · 29 citations · 27 references
Natural SciencesMaterials EngineeringMaterials ScienceCeramic MaterialsCeramicsMechanical Behavior Of MaterialsAluminum OxidesComposite MaterialsDuctilityHigh-temperature MaterialsStrength Of MaterialsStructural CeramicsAluminaAlumina CeramicsAlumina-based Ceramic CompositesFlow StressGrain BoundariesHigh-temperature Performance Of Ceramic CompositesZirconiaZirconia Materials
Layered composites of alternate layers of pure Al 2 O 3 (thickness of 125 μ m) and 85 vol% Al 2 O 3 ‐15 vol% ZrO 2 that was stabilized with 3 mol% Y 2 O 3 (thickness of 400 μ m) were obtained by sequential slip casting and then fired at either 1550° or 1700°C. Constant‐strain‐rate tests were conducted on these materials in air at 1400°C at an initial strain rate of 2 × 10 ‐5 s ‐1 . The load axis was applied both parallel and perpendicular to the layer interfaces. Catastrophic failure occurred for the composite that was fired at 1700°C, because of the coalescence of cavities that had developed in grain boundaries of the Al 2 O 3 layers. In comparison, the composite that was fired at 1550°C demonstrated the ductility of the Al 2 O 3 +YTZP layer, but at a flow stress level that was determined by the Al 2 O 3 layer.
27
A simple way to make tough ceramics
W.J. Clegg, K. Kendall, Neil McN. Alford et al. · Nature · 1990 · 838 citations
Natural Sciences, Materials Engineering, Materials Science +13