Journal of Applied Physics · 1993 · 23 citations · 7 references
Natural SciencesMaterials EngineeringMaterials ScienceMagnetic MaterialsMetallic MaterialsMetallurgyAlloysFerromagnetic MaterialsFerromagnetismMagnetic AnisotropyMagnetic Properties Of SolidsMagnetism In SolidsBonded MagnetsCoercivityCoercivity EnhancementEnergy DensityFerromagnetic CeramicsMagnetic PropertiesPowder Metallurgy Of MagnetsSaturation Magnetization
Hard magnetic Sm2Fe17Nx alloy powders with a coercivity of 5.6 kA/cm and a remanent polarization of 1 T, related to the density of 7.7 g/cm3, could be achieved by a combined heat treatment in hydrogen atmosphere and a successive nitrogenation. During nitrogenation SmFe3 and SmFe2 constituents decompose into SmN and αFe immediately. The density of die-pressed anisotropic Sm2Fe17Nx magnets containing 5 wt % Zn amounts to ∼5 g/cm3 and increases to 5.25 g/cm3 for additions of 20 wt % Zn. After annealing at 390 °C for 10 h, the remanent polarization of 0.66 T and the coercivity of 8.8 kA/cm result in a maximal energy density of 67 kJ/m3. Annealing at temperatures of ∼420 °C achieves additional αFe due to a decomposition of Sm2Fe17Nx by Zn: Sm2Fe17Nx+Zn→Sm2FeZn2+αFe+N2. Additions of 10 wt % Sn result in a density of 4.6 g/cm3 of isostatically compacted magnets. The remanent polarization amounts to ∼0.6 T, but the coercivity Hcj of ∼4 kA/cm is inferior to Zn-bonded Sm2Fe17Nx magnets.
7
High coercivity in Sm2Fe17N<i>x</i> magnets
K. Schnitzke, L. Schultz, J. Wecker et al. · Applied Physics Letters · 1990 · 256 citations
Natural Sciences, Materials Engineering, Materials Science +17
Nitrogenation of R2Fe17 compounds: <i>R</i>=rare earth
J. M. D. Coey, J.F. Lawler, Hong Sun et al. · Journal of Applied Physics · 1991 · 141 citations
Natural Sciences, Materials Engineering, Materials Science +15
Metal-bonded Sm2Fe17-N-type magnets
Min Huang, L. Y. Zhang, B. M. et al. · Journal of Applied Physics · 1991 · 81 citations
Natural Sciences, Materials Engineering, Materials Science +17