Thermoelectric instability in Pd within the elemental thermocouple Pt/Pd

R E Bentley

Measurement Science and Technology · 2001 · 16 citations · 11 references

Concepts

Abstract

A scanning facility was used to study the thermoelectric behaviour of Pd wires from three sources. The facility measured changes in Seebeck emf along a 560 mm length of each of three wires, relative to a fourth, by moving them through a 50 mm long, emf-producing zone into a uniform-temperature region at 250 °C. Both reversible and irreversible changes were measured. The most significant is reversible change, which peaks at -1.6 µV after 200 h of annealing at about 720 °C, when measured at 250 °C. However, the magnitude and sign of the peak is a function of the temperature at which it is measured. Possible mechanisms to account for reversible change were examined and oxidation of impurities was shown to be the most likely.

References

11