Journal of The Electrochemical Society · 2010 · 10 citations · 13 references
Natural SciencesMaterials EngineeringMaterials ScienceInorganic ChemistryMaterials ChemistryOptical MaterialsCrystal ChemistryCrystalline MaterialsLuminescent MaterialsOptical CeramicsPerovskite MaterialsRare-earth-doped MaterialsAnnealingInorganic PhosphorsLow-temperature SynthesisPhosphor MaterialsPhosphorescent MaterialsPhosphorsPhotoluminescenceRare-earth-doped Luminescent Materials
A or flux was added to a mixture of BaS, EuS, Al, and S to synthesize a Eu-doped cubic phosphor. The formation temperature of the cubic phase was lowered to , which was below the temperature of a case without a flux. To improve the crystallinity and color purity, a two-step annealing process that involved low temperature annealing ( for and for ) was proposed for a uniform immersion of a flux into a starting mixture and a high temperature annealing for the formation of . The phosphor synthesized by the two-step process with a 2 wt % flux showed a distinct cubic phase and a strong photoluminescence (PL) intensity at 475 nm. The PL intensity was 6.6 times stronger than that of the phosphor without a flux. The phosphor synthesized with a flux showed only an orthorhombic phase, while direct annealing at 600° with the flux showed a mixture of cubic and orthorhombic phases. The role of the fluxes in the formation mechanism of the cubic and orthorhombic phases was described.
13