Evaluating the durability of wood-based panels using thickness swelling results from accelerated aging treatments

Yoichi Kojima, H. Norita, Shigehiko Suzuki

Forest Products Journal · 2009 · 29 citations · 0 references

Concepts

Abstract

Durability of wood-based panels was evaluated by comparing thickness swelling (TS) results from five laboratory-accelerated aging tests with the TS results from panels that had experienced 2 years of outdoor exposure in Shizuoka City, Central Honshu, Japan. In each accelerated aging test, the total TS of phenol-formaldehyde (PF) resin bonded panels were higher than that of isocyanate resin diphenylmethane diisocyanate (MDI) bonded panels. The panels could be divided into two groups based on the results of non-linear least-squares regression analysis of the rates of increase in TS. The Shizuoka 2-year outdoor exposure test resulted in the TS of oriented strandboard (OSB) made from aspen exceeding 15 percent; TS of OSB made from pine and particleboard bonded with PF resin was about percent. On the other hand, TS of the tested plywood and medium density fiberboard remained below 3 percent over the 2 years. Calculation of mean TS for all of the panels tested allowed comparison of the severity of aging between the accelerated test methods and outdoor exposure. Of the standard methods, the ASTM six-cycle test was the most severe, with the 2-year outdoor exposure proving no harsher than any of the accelerated aging procedures used.