Low‐Temperature Sintering of La(Ca)CrO <sub>3</sub> Powder Prepared through the Combustion Process

Sathi R Nair, R.D. Purohit, A. K. Tyagi, P.K. Sinha, Beant Prakash Sharma

Journal of the American Ceramic Society · 2007 · 14 citations · 28 references

Concepts

Abstract

Ultrafine La(Ca)CrO 3 (LCC) powder was prepared through the glycine–nitrate gel combustion process. It was shown for the first time that the use of relatively inexpensive CrO 3 as a starting material for chromium has potential for the bulk preparation of sinter‐active LCC powder. As‐prepared powder, when calcined at 700°C, resulted in LCC along with a small amount of CaCrO 4 . The calcined powder was found to be composed of soft agglomerates with a particle size of ≈70–290 nm. The cold pressing and sintering of the calcined powder at 1200°C resulted in the mono‐phasic La 0.7 Ca 0.3 CrO 3 with density ≈98% of its theoretical value. This is the lowest sintering temperature ever reported for La 0.7 Ca 0.3 CrO 3 . The conductivity of the sintered La 0.7 Ca 0.3 CrO 3 at 1000°C was found to be ≈57 S/cm in air. The sintering and electrical behavior achieved for La 0.7 Ca 0.3 CrO 3 may find application as an interconnect material for high‐temperature solid oxide fuel cells if problems with chemical expansion and poor conductivity in fuel can be overcome.

References

28