Oxides on the Silver Electrode

Charles P. Wales, Jeanne Burbank

Journal of The Electrochemical Society · 1965 · 16 citations · 0 references

Concepts

Abstract

Silver electrodes were examined in 20–50% using a cell permitting simultaneous x‐ray diffraction and electrochemical studies. Highly oriented smooth rolled sheet Ag developed randomly oriented Ag on its surface during early cycles. Charge‐discharge capacity increased to a maximum as surface area increased. crystal size and amount formed varied inversely with charging c. d. High charge rates gave tight coatings of small crystals that limited further oxidation. Reactions took place initially at the outer surface of the electrode. Oxidation to and and reduction to and Ag occurred by formation of distinct crystals rather than expansion or contraction of preexisting crystal lattices. Discharge capacity at the potential plateau depended more on surface area than on quantity of . A slow discharge produced smoother Ag surfaces, lowering capacity of the next cycle. There was never evidence of a suboxide, oxidation state higher than , solid solution, or alloy of oxygen and silver.