Electrochemical Noise Measurements of Steel Corrosion in the Molten NaCl-K[sub 2]SO[sub 4] System

F. Cappeln, Niels J. Bjerrum, Irina Petrushina

Journal of The Electrochemical Society · 2005 · 18 citations · 17 references

DOIFull text

Open access

Concepts

Abstract

Electrochemical noise measurements have been carried out on AISI347, 10CrMo910, 15Mo3, and X20CrMoV121 steels in molten NaCl-K 2 SO 4 at 630C. Different types of current noise have been identified for pitting, intergranular and peeling corrosion. The corrosion mechanism was the so-called active corrosion i.e., the corrosion proceeds with no passivation due to the influence of chlorine, characterized by the formation of volatile metal chlorides as a primary corrosion product. It was found possible to obtain an empirical separation of general and intergranular corrosion using kurtosis a statistical parameter calculated from the electrochemical noise data. It was found that average kurtosis values above 6 indicated intergranular corrosion and average values below 6 indicated general corrosion. The response time for localized corrosion detection in in-plant monitoring was approximately 90 min on this basis. Approximate values of polarization resistances of AISI347 and 15Mo3 steels were determined to be 250 and 100 cm 2 , respectively.

References

17