Enthalpy of polymerisation of 7‐oxabicyclo[2.2.1]heptane, and <i>exo</i>‐ and <i>endo</i>‐2‐methyl‐7‐oxabicyclo[2.2.1]heptane

F. Andruzzi, G. Pilcher, Yogesh Virmani, P. H. Plesch

Die Makromolekulare Chemie · 1977 · 11 citations · 10 references

Concepts

Abstract

Abstract The enthalpies of combustion of poly(oxy‐1,4‐cyclohexylene) formed from 7‐oxabicyclo[2.2.1]heptane ( 1 ) and of its derivatives formed from exo ‐ and endo ‐3‐methyl‐7‐oxabicyclo[2.2.1]heptane ( 2a and 2b ) have been measured. From literature values for the enthalpies of combustion of the liquid monomers, the enthalpies of polymerisation have been derived: −ΔH (1→c)=44,3±1,9, 49,7±2,6, and 45.4±3,1 kJ mol −1 , respectively. The results indicate a minimum strain energy in these polymers of ca. 15 kJ mol −1 . The estimated entropies of polymerisation yield ceiling temperatures of 320, 240, 200°C respectively for the three bicyclic ethers.—The reasons for the discrepancy between our present −ΔH (1→c) for the endo compound and that previously reported 2 , are explained.

References

10