Journal of Applied Physics · 2002 · 84 citations · 18 references
Natural SciencesMaterials EngineeringMaterials ScienceMagnetic MaterialsMaterials ChemistryNanomaterialsIron OxidesMagnetic NanomaterialsMagnetic OxidesMagnetic Properties Of SolidsMagnetization ProcessesMetal Oxide NanomaterialsAnnealingMagnetic Grain SizeMagnetic Oxide NanoparticlesMagnetic PropertiesNanoparticlesSize EffectsSize-dependent Magnetic Properties
Sonochemically synthesized Fe2O3 nanoparticles were annealed in air or in vacuum while their magnetization was continuously recorded. Annealing in vacuum at temperatures Ta between 240 and 450 °C produced nanophases of γ-Fe2O3 with average particle size ranging from 4 to 14 nm, depending on Ta. Phase transformation into α-Fe2O3 occurred directly by annealing in air, or via an intermediate Fe3O4 phase by annealing in vacuum at temperatures higher than 450 °C. Mapping the correlation between the magnetic properties and the annealing conditions, enables control of the annealing process to obtain nanocrystals of γ-Fe2O3, α-Fe2O3, or Fe3O4 with different particle size and magnetic properties.
18