TIME DEPENDENCE OF CATHODIC PROPERTIES OF MATERIALS IN SEAWATER - STAINLESS STEEL, TITANIUM, PLATINUM AND 90/10 CU-NI

R Holthe, Einar Bardal, Per Olav Gartland

Materials performance · 1989 · 10 citations · 0 references

Concepts

Abstract

This article describes how the cathodic efficiency of stainless steels, titanium, platinum and 90/10 Cu-Ni increases during the first weeks of exposure in natural seawater due to a catalytic action of a microbial slime layer. The increase in cathodic efficiency of stainless steels has been studied for various polarisation potentials, temperatures and flow rates. At temperatures below 30 C and any fixed potential in the region from 200 to -600 mV SCE, the cathodic current density on stainless steels increases strongly after several days or a few weeks of exposure. In the potential range -200 to -1200 mV SCE the lowest current density is found at -1000 mV SCE. In the upper potential region, titanium, platinum and 90/10 Cu-Ni also show an increase in cathodic current density during the same period. The catalytic effect of the biofilm vanishes when the temperature is raised above 30 C. The increased cathodic efficiency leads to a shift in the free corrosion potential, and the initiation and propagation of crevice corrosion are favoured. Current demand for cathodic protection and galvanic corrosion rates on less noble materials in galvanic contact with stainless steels and titanium are increased.