Anomalously High Remanence in (γ−Fe2O3)1−<i>x</i>· (α−Fe2O3)<i>x</i> Particles

B. Gustard, W. J. Schuele

Journal of Applied Physics · 1966 · 21 citations · 1 references

Concepts

Abstract

The remanent magnetization of acicular γ−Fe2O3 particles partially converted to hematite by heating in air was measured after saturation and ac demagnetization using a vibrating-sample magnetometer. It is possible that commercial γ−Fe2O3 recording tapes could undergo this partial conversion which may result in a deterioration of their magnetic properties. The complete composition range from pure γ Fe2O3 to hematite was studied. The composition was determined by interpolation of the saturation magnetization of the sample and of the values for pure γ Fe2O3 and hematite. The remanent magnetization increases as a function of hematite composition. At 90% hematite there is a peak in the remanent magnetization which is a factor of 2 greater than the remanence of the two components. The coercivity was approximately constant, 320 Oe, as a function of composition except that pure hematite had a value of 635 Oe. Partially converted particles were examined using dark-field electron microscopy to indicate the method of conversion.

References

1