Ferroelectrics · 1981 · 51 citations · 3 references
Natural SciencesMaterials EngineeringMaterials ScienceCeramic MaterialsCeramicsMaterials ChemistryCeramic CompositesCurie TemperatureGlass MaterialsSinteringThermal Properties Of CeramicsThermodynamics Of CeramicsBarium Titanate CeramicsGlass-ceramicsLiquid-phase SinteringSintering Behavior
Abstract BaTiO3 has been sintered at 1000-1100°C for periods from 1/6 to 2 hours with 10-20 wt% glass of 74mole% Bi2O3 - 26% B2O3 composition. The resulting composites, consisting of BaTiO3 grains surrounded by a glass, show ϵRT=1300-1500 and ϵmax=2500. The Curie temperature is nearly unaffected by the amount of the glass content.
3